Stainless steel EP pipes generally encounter various problems during the processing. Especially for some stainless steel pipe processing manufacturers with relatively immature technology, not only are they likely to produce scrap steel pipes, but the properties of the secondary processed stainless steel pipes are significantly reduced. In this regard, Huzhou Zhongrui Precision Technology Co., Ltd. has compiled and listed some easily encountered problems for your reference:
The welding seam defects are serious, and manual mechanical grinding is used to make up for them. The resulting grinding marks will cause the surface to be uneven and unsightly.
2. Surface inconsistency:
Only pickling and passivating the welds will also cause the surface to be uneven and unsightly.
3. Scratches are difficult to remove:
Overall pickling and passivation cannot remove various scratches produced during processing, and cannot clean carbon steel, splashes and other impurities that adhere to the surface of stainless steel due to scratches and welding spatter, resulting in the presence of impurities in corrosive media. Chemical corrosion or electrochemical reaction occurs under certain conditions and causes corrosion. Seamless steel pipe price, seamless pipe, oil casing, 12cr1mov, seamless steel pipe price, precision seamless steel pipe, 16mn seamless pipe, 15crmo alloy pipe, q345b seamless pipe, q345b seamless pipe, line pipe, 35crmo steel pipe , 12cr1mov alloy pipe, high pressure alloy pipe, Chongqing seamless pipe, bearing steel pipe, alloy pipe, precision seamless steel pipe, 15crmo steel pipe…
4. Uneven polishing and passivation:
After manual grinding and polishing, pickling and passivation treatment are performed. For workpieces with larger areas, it is difficult to achieve a uniform and consistent treatment effect, and an ideal uniform surface layer cannot be obtained. Moreover, labor costs and auxiliary material costs are also high.
5. Limited pickling capacity:
Pickling passivation paste is not foolproof. It is difficult to remove the black oxide scale produced by plasma cutting and flame cutting.
6. The scratches caused by elements are serious:
During lifting, transportation and structural processing, scratches caused by human factors such as bumping, dragging and hammering are relatively serious, which makes surface treatment more difficult and is also an important reason for rust after treatment.
article souce: https://www.zrctube.com/news/problems-easily-encountered-during-the-processing-of-stainless-steel-ep-pipes/
Media Contact
Company Name: Huzhou Zhongrui Cleaning Technology Co., Ltd.
Email: Send Email
Country: China
Website: https://www.zrctube.com/